Whenever very high radial shrinkage (up to 50% or more) is required, the Drawing
Process can be used. This simply requires axial tension and stretching of the tube
while it is being heated. Over 50% diameter reduction can be achieved at temperatures
below 100°C (212°F). Higher diameter reductions can be achieved at higher temperatures,
up to about 190°C (374°F).
View Process